This research aims to evaluate the strength development and microstructure of a green mortar produced from waste red brick powder (WRP) as a partial cement replacement. The mortar samples were prepared with various WRP content of 0%, 10%, 20%, 30%, and 40% of total binder weight, and the w/b was fixed at 0.4. The fresh properties were checked by flowability and fresh unit weight. While the compressive strength was conducted up to 28 days. The mortar samples exhibited a reduction in flowability and unit weight with increasing WRP content. The incorporation of 10%-20% WRP improved the compressive strength of mortar samples at 28-day, while the compressive strength reduced with higher WRP content (30%- 40%). The C-S-H/CaCO3 gel, Ca(OH)2 and ettringite were hydration products of WRP mortar samples. The incorporation with WRP significantly reduced the Ca(OH)2 content.
Tạp chí khoa học Trường Đại học Cần Thơ
Lầu 4, Nhà Điều Hành, Khu II, đường 3/2, P. Xuân Khánh, Q. Ninh Kiều, TP. Cần Thơ
Điện thoại: (0292) 3 872 157; Email: tapchidhct@ctu.edu.vn
Chương trình chạy tốt nhất trên trình duyệt IE 9+ & FF 16+, độ phân giải màn hình 1024x768 trở lên