This research aims to evaluate the strength development and microstructure of a green mortar produced from waste red brick powder (WRP) as a partial cement replacement. The mortar samples were prepared with various WRP content of 0%, 10%, 20%, 30%, and 40% of total binder weight, and the w/b was fixed at 0.4. The fresh properties were checked by flowability and fresh unit weight. While the compressive strength was conducted up to 28 days. The mortar samples exhibited a reduction in flowability and unit weight with increasing WRP content. The incorporation of 10%-20% WRP improved the compressive strength of mortar samples at 28-day, while the compressive strength reduced with higher WRP content (30%- 40%). The C-S-H/CaCO3 gel, Ca(OH)2 and ettringite were hydration products of WRP mortar samples. The incorporation with WRP significantly reduced the Ca(OH)2 content.
Tạp chí: The Fourth International Conference on Communication, Computing and Electronics Systems . Lecture Notes in Electrical Engineering, vol 977. Springer. Coimbatore, India. September 15-16, 2022
Tạp chí: Association for Computational Linguistics (ACL 2023), In Findings of the Association for Computational Linguistics: ACL 2023, Toronto, Canada, 2023
Tạp chí khoa học Trường Đại học Cần Thơ
Lầu 4, Nhà Điều Hành, Khu II, đường 3/2, P. Xuân Khánh, Q. Ninh Kiều, TP. Cần Thơ
Điện thoại: (0292) 3 872 157; Email: tapchidhct@ctu.edu.vn
Chương trình chạy tốt nhất trên trình duyệt IE 9+ & FF 16+, độ phân giải màn hình 1024x768 trở lên